Test Film with 510 Pyro

Testing 8 different films, all 120 in a stand development 1:500 in 510 Pyro Developer… film was exposed at +3, +2, +1, Box Speed, -1 and -2 to see developer / film latitude combination… have seen some pretty amazing results with this developer…. more later…. (Films Tested: Rollei RPX 400, Bergger Pancro 400, Ilford HP5+, Ilford Delta 3200, Ilford Pan F+, Ilford FP4+, Fomapan 100 and Kodak 400TX ).

Many thanks to my friend Dan for introducing me to this developer and to Jay DeFehr on getting this up and running and for being such a helpful source of knowledge.

Viva la Revolution- Steve

 

5 thoughts on “Test Film with 510 Pyro

    1. for 510 everything is at 70F and mixed with distilled water… 5 min pre wet, developer is agitated for the first 30 seconds at 2 inversions per 5 seconds…. then at 30 minutes the film is agitated again for two slow inversion and dumped at 1 hour… this is a at 1:500 dilution.

Leave a Reply

Fill in your details below or click an icon to log in:

WordPress.com Logo

You are commenting using your WordPress.com account. Log Out /  Change )

Facebook photo

You are commenting using your Facebook account. Log Out /  Change )

Connecting to %s